Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
Niche Polymer PA66GI14BK Nylon 66, 14% Glass Fiber Filled, Impact Modified Information provided by Niche Polymer |
|||
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
Polymer Resources TP-HG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy Polybutylene Terephthalate, 30% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GB40 BK 40% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GB40 HS BK 40% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: BlackInforma.. |
|||
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF13 SL2 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and Silicone LubricantFeatures: Lubricated and Heat StabilizedInformation pr.. |
|||
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
Techmer ES Electrablend® PA6/6 03001 Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Impact Modifier and Heat StabilizerFeatures: Electrically Conductive, Impact Modified and Heat Stab.. |
|||
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
Chase Plastics CP Pryme® N140MGHL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
Chase Plastics CP Pryme® N340MGL (DAM) Nylon 6 (Utility Grade), 40% Mineral/Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Strength | 165 MPa | 24000 psi | ASTM D790 |
Ensinger Tecapeek® XP-112 Compression Molded PEEK Compound, 20% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |