Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 86.25 MPa | 12510 psi | ASTM D-790 |
Plaskolite Optix® CP - 924 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 86.25 MPa | 12510 psi | ASTM D-790 |
Plaskolite West Optix® CP - 924 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |