Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 83.6 MPa | 12100 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87180 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Flexural Strength | 83.6 MPa | 12100 psi | ASTM D790-03 |
Objet FullCure® 840 Vero Blue Resin for Rapid Prototyping Information provided by American Precision Prototyping, LLC |
|||
Flexural Strength | 83.6 MPa | 12100 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L6181 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |