Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 68.40 MPa | 9921 psi | ASTM D790 |
PolyOne Therma-Tech™ NJC-5000 TC NATURAL Nylon 12
(discontinued **) Information provided by PolyOne Corporation. |
|||
Flexural Strength | 68.40 MPa | 9921 psi | ASTM D790 |
PolyOne Therma-Tech™ NJC-6500 Nylon 12
(discontinued **) PolyOne First ChoiceInformation provided by PolyOne Corporation. |