Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 369 MPa | 53500 psi | ASTM D-790 |
PlastiComp Velocity® LGF50-PA66 High Flow Nylon 66, 50% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Flexural Strength | 369 MPa | 53500 psi | |
PCC-Advanced Forming Technology 63% AlSiC Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
Flexural Strength | 369 MPa | 53500 psi | ASTM D-790 |
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In.. |