Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 273 MPa | 39600 psi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
Flexural Strength | 273 MPa | 39600 psi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Flexural Strength | 273 MPa | 39600 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP QFL17RS PA 6/10 LNP LUBRICOMP* QFL17RS is a compound based on Nylon 6/10 resin containing 35% Glass Fiber, 5% PTFE. Added features of this material include: Easy Release, Heat Stabilized, Wear Resistant. |
|||
Flexural Strength | 273 MPa | 39600 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Verton RV008ESV_GY7E072 PA 66 Preliminary data for 40% long glass fiber filled, single color pellet gray, PA66This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 273 MPa | 39600 psi | Machine; IPC TM-650 2.4.18.3 |
Arlon MULTICLAD™ HF Halogen-Free Low-Loss Laminate and Prepreg System MULTICLAD™ HF represents the next generation low-loss thermoset and prepreg system for high-speed and high-frequency printed circuit boards. This technology combines a low-loss, high reliability t.. |