Mechanical Properties Metric English Comments
Flexural Strength 2450 MPa
355000 psi
China Tungsten YG20 Tungsten Carbide for Dies and Wear Part Making
For fabricating of stamping dies for watch parts, spring plates of musical instruments, batters jars, small sized steel balls, screws, screwcaps, etc; and for press plates for hot rolling of twist d..
Flexural Strength >= 2450 MPa
>= 355000 psi
China Tungsten ZY31 Tungsten Carbide for Mining Purposes
High impact toughness, for hi-speed wire mills for primary and intermediate rolling of mild wire rods.Information provided by China Tungsten