Material Notes:
For fabricating of stamping dies for watch parts, spring plates of musical instruments, batters jars, small sized steel balls, screws, screwcaps, etc; and for press plates for hot rolling of twist drill bitsInformation provided by China Tungsten
Physical Properties Metric English Comments
Density 13.4 - 13.7 g/cc
0.484 - 0.495 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A >= 85
>= 85
Flexural Strength 2450 MPa
355000 psi