Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1.80 MPa | 261 psi | @ 15 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SF-101H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 1.80 MPa | 261 psi | @ 15 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SG-101 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 1.80 MPa | 261 psi | @ 15 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SG-201 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 1.80 MPa | 261 psi | @ 15 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SG-202 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 1.80 MPa | 261 psi | @ 15 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SF-101H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 1.80 MPa | 261 psi | @ 15 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SG-101 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 1.80 MPa | 261 psi | @ 15 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SG-201 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 1.80 MPa | 261 psi | @ 15 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SG-202 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |