Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Modulus | 0.0986 GPa | 14.3 ksi | ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |