Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Modulus | 0.0372 GPa | 5.40 ksi | ASTM D1043 |
PolyOne Geon™ Vinyl Flexible A7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Interior compound used primarily in transparent applications. This product is registered under UL 94 HB specifications @ 3.0 and 1.5 mm. thickness and all colors.Information provided by PolyOne |
|||
Clash Berg Modulus | 0.0372 GPa @Temperature -35.0 °C |
5.40 ksi @Temperature -31.0 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible 86280 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |