Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 65.6 MPa @Strain 0.750 %, Temperature 40.0 °C |
9510 psi @Strain 0.750 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 65.6 MPa @Strain 0.750 %, Temperature 40.0 °C |
9510 psi @Strain 0.750 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Tensile Stress | 65.6 MPa @Strain 15.0 %, Temperature 23.0 °C |
9510 psi @Strain 15.0 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub.. |
|||
Tensile Stress | 65.6 MPa @Strain 15.0 %, Temperature 23.0 °C |
9510 psi @Strain 15.0 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)