Mechanical Properties Metric English Comments
Tensile Stress 57.07 MPa

@Strain 4.70 %,
Temperature 150 °C
8277 psi

@Strain 4.70 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)  (Unverified Data**)
20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Stress 57.07 MPa

@Strain 0.610 %,
Temperature 40.0 °C
8277 psi

@Strain 0.610 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6  (Unverified Data**)
50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc..
Tensile Stress 57.07 MPa

@Strain 3.40 %,
Temperature 150 °C
8277 psi

@Strain 3.40 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon  (Unverified Data**)
Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve..