Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.93 MPa @Strain 300 % |
715 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P2775 TPE, PP Overmold or Standalone use Characteristics: Soft, flexible feelExcellent grip characteristicsGood weatherabilityGood compression setEasy processability and colorabilityAvailable FDA and medical gradesAvailable translucent gra.. |
|||
Tensile Stress | 4.93 MPa @Strain 300 % |
715 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® D6770 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Stress | 4.93 MPa @Strain 20.43 %, Temperature 23.0 °C |
715 psi @Strain 20.43 %, Temperature 73.4 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 4.93 MPa @Strain 6.00 %, Temperature 90.0 °C |
715 psi @Strain 6.00 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 4.93 MPa @Strain 6.00 %, Temperature 90.0 °C |
715 psi @Strain 6.00 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |