Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 49.0 MPa @Strain 1.50 %, Temperature -40.0 °C |
7110 psi @Strain 1.50 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Tensile Stress | 49.0 MPa @Strain 1.25 %, Temperature 90.0 °C |
7110 psi @Strain 1.25 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G35HSLRA4 BK267 is a 35% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection m.. |
|||
Tensile Stress | 49.0 MPa @Strain 1.45 %, Temperature 90.0 °C |
7110 psi @Strain 1.45 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR NC010 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Tensile Stress | 49.0 MPa @Strain 50.0 %, Temperature 23.0 °C |
7110 psi @Strain 50.0 %, Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
Tensile Stress | 49.0 MPa @Strain 0.0500 %, Temperature 1204 °C |
7110 psi @Strain 0.0500 %, Temperature 2199 °F |
|
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |