Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 44.9 MPa @Strain 2.20 %, Temperature 23.0 °C |
6510 psi @Strain 2.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub.. |
|||
Tensile Stress | 44.9 MPa @Strain 12.1 %, Temperature 0.000 °C |
6510 psi @Strain 12.1 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Tensile Stress | 44.9 MPa @Strain 2.20 %, Temperature 23.0 °C |
6510 psi @Strain 2.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing .. |
|||
Tensile Stress | 44.9 MPa @Strain 6.28 %, Temperature -20.0 °C |
6510 psi @Strain 6.28 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 44.9 MPa @Strain 0.460 %, Temperature 0.000 °C |
6510 psi @Strain 0.460 %, Temperature 32.0 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Tensile Stress | 44.9 MPa @Strain 21.2 %, Temperature 40.0 °C |
6510 psi @Strain 21.2 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 44.9 MPa @Strain 7.40 %, Temperature 23.0 °C |
6510 psi @Strain 7.40 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |