Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.98 MPa @Strain 100 % |
577 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P2775 TPE, PP Overmold or Standalone use Characteristics: Soft, flexible feelExcellent grip characteristicsGood weatherabilityGood compression setEasy processability and colorabilityAvailable FDA and medical gradesAvailable translucent gra.. |
|||
Tensile Stress | 3.98 MPa @Strain 76.93 %, Temperature 90.0 °C |
577 psi @Strain 76.93 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.98 MPa @Strain 86.92 %, Temperature 100 °C |
577 psi @Strain 86.92 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.98 MPa @Strain 6.86 %, Temperature 60.0 °C |
577 psi @Strain 6.86 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 3.98 MPa @Strain 60.25 %, Temperature 180 °C |
577 psi @Strain 60.25 %, Temperature 356 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |