Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 39.2 MPa @Strain 14.8 %, Temperature 23.0 °C |
5690 psi @Strain 14.8 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Tensile Stress | 39.2 MPa @Strain 1.00 %, Temperature 23.0 °C |
5690 psi @Strain 1.00 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Tensile Stress | 39.23 MPa @Strain 0.400 %, Temperature 40.0 °C |
5690 psi @Strain 0.400 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 39.23 MPa @Strain 0.400 %, Temperature 100 °C |
5690 psi @Strain 0.400 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G45HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G45HSL NC010 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide.. |
|||
Tensile Stress | 39.23 MPa @Strain 2.53541 %, Temperature 160 °C |
5690 psi @Strain 2.53541 %, Temperature 320 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |