Mechanical Properties Metric English Comments
Tensile Stress 37.95 MPa

@Strain 0.650 %,
Temperature 90.0 °C
5504 psi

@Strain 0.650 %,
Temperature 194 °F
ISO 527
DuPont Performance Polymers Crastin® SK608 BK509 PBT  (Unverified Data**)
Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers