Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.79 MPa @Strain 300 % |
550 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3760 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.79 MPa @Strain 300 % |
550 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3770 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.79 MPa @Strain 100 % |
550 psi @Strain 100 % |
ASTM D412 Method A |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |
|||
Tensile Stress | 3.79 MPa @Strain 300 % |
550 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TELC 302 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Stress | 3.79 MPa @Strain 0.100 %, Temperature 150 °C |
550 psi @Strain 0.100 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc.. |