Mechanical Properties Metric English Comments
Tensile Stress 30.9 MPa

@Strain 4.60 %,
Temperature 90.0 °C
4480 psi

@Strain 4.60 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low..
Tensile Stress 30.9 MPa

@Strain 1.10 %,
Temperature 23.0 °C
4480 psi

@Strain 1.10 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..
Tensile Stress 30.9 MPa

@Strain 1.20 %,
Temperature 23.0 °C
4480 psi

@Strain 1.20 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..
Copyright © lookpolymers.com All Rights Reserved