Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.70 MPa @Strain 100 % |
392 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S FR 70A-3S1890 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tensile Stress | 2.70 MPa @Strain 0.000 %, Temperature -20.0 °C |
392 psi @Strain 0.000 %, Temperature -4.00 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |
|||
Tensile Stress | 2.70 MPa @Strain 17.6 %, Temperature 150 °C |
392 psi @Strain 17.6 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.70 MPa @Strain 300 % |
392 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G50A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.70 MPa @Strain 300 % |
392 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G50A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.70 MPa @Strain 300 % |
392 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G50D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.70 MPa @Strain 300 % |
392 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.70 MPa @Strain 100 % |
392 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.70 MPa @Strain 100 % |
392 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P70A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |