Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.69 MPa @Strain 100 %, Temperature 23.0 °C |
390 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ HC MT307 Thermoplastic Elastomer (TPE) Versaflex™ HC MT307 is an extrudable, autoclavable TPE developed for medical tubing applications in healthcare. New Product. Commercial specifications have not been established. - Autoclavable - Fl.. |
|||
Tensile Stress | 2.69 MPa @Strain 100 % |
390 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P2665 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.69 MPa @Strain 100 % |
390 psi @Strain 100 % |
|
NEU NeuSoft™ 602-60A Ester TPU / SBC blend |
|||
Tensile Stress | 2.69 MPa @Strain 100 %, Temperature 23.0 °C |
390 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Tensile Stress | 2.69 MPa @Strain 100 %, Temperature 23.0 °C |
390 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - .. |
|||
Tensile Stress | 2.69 MPa @Strain 100 % |
390 psi @Strain 100 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-2065 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Stress | 2.69 MPa @Strain 300 %, Temperature 23.0 °C |
390 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over.. |
|||
Tensile Stress | 2.69 MPa @Strain 300 % |
390 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL-88-N873C BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Stress | 2.69 MPa @Strain 149.53 %, Temperature 120 °C |
390 psi @Strain 149.53 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.69 MPa @Strain 6.08 %, Temperature 40.0 °C |
390 psi @Strain 6.08 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |