Mechanical Properties Metric English Comments
Tensile Stress 19.5 MPa

@Strain 0.600 %,
Temperature 23.0 °C
2830 psi

@Strain 0.600 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by ..
Tensile Stress 19.5 MPa

@Strain 0.600 %,
Temperature 23.0 °C
2830 psi

@Strain 0.600 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Tensile Stress 19.5 MPa

@Strain 5.00 %,
Temperature -40.0 °C
2830 psi

@Strain 5.00 %,
Temperature -40.0 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 19.5 MPa

@Strain 10.0 %
2830 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® CM600-V TPC-ES FR
Extrusion, Flame Retardant (Halogen free)
Tensile Stress 19.5 MPa

@Strain 0.210 %,
Temperature 23.0 °C
2830 psi

@Strain 0.210 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti..
Copyright © lookpolymers.com All Rights Reserved