Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 14.12 MPa @Strain 133.7 %, Temperature 100 °C |
2048 psi @Strain 133.7 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 14.12 MPa @Strain 39.22 %, Temperature 90.0 °C |
2048 psi @Strain 39.22 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 14.12 MPa @Strain 10.0 %, Temperature -40.0 °C |
2048 psi @Strain 10.0 %, Temperature -40.0 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |