Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 14.0 MPa @Strain 50.0 %, Temperature 23.0 °C |
2030 psi @Strain 50.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET
(Unverified Data**) Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,.. |
|||
Tensile Stress | 14.0 MPa @Strain 2.00 %, Temperature 60.0 °C |
2030 psi @Strain 2.00 %, Temperature 140 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 14.0 MPa @Strain 5.00 % |
2030 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 14.0 MPa @Strain 100 % |
2030 psi @Strain 100 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Tensile Stress | 14.0 MPa @Strain 10.0 %, Temperature 23.0 °C |
2030 psi @Strain 10.0 %, Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Tensile Stress | 14.0 MPa @Strain 100 % |
2030 psi @Strain 100 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |
|||
Tensile Stress | 14.0 MPa @Strain 50.0 % |
2030 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi.. |
|||
Tensile Stress | 14.0 MPa @Strain 0.530 %, Temperature 0.000 °C |
2030 psi @Strain 0.530 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 14.0 MPa @Strain 100 % |
2030 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 14.0 MPa @Strain 300 % |
2030 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer Zythane™ 4080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 14.0 MPa @Strain 100 % |
2030 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 6050D Thermoplastic Polyurethane Elastomer Zythane™ 6050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 14.0 MPa @Strain 100 % |
2030 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | >= 14.0 MPa @Strain 100 % |
>= 2030 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 764D PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tensile Stress | 14.0 MPa @Strain 100 % |
2030 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® EB464-01 TPC-ET Antisqueak Blow Molding Grade |
|||
Tensile Stress | 14.0 MPa @Strain 0.450 %, Temperature 0.000 °C |
2030 psi @Strain 0.450 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 14.0 MPa @Strain 300 % |
2030 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |