Polymer Property : Tensile Stress = 1600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 11.0 MPa

@Strain 300 %
1600 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3892 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 11.0 MPa

@Strain 300 %
1600 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9190 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun..
Tensile Stress 11.0 MPa

@Strain 100 %
1600 psi

@Strain 100 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 11.0 MPa

@Strain 10.0 %
1600 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 11.0 MPa

@Strain 10.0 %,
Temperature 23.0 °C
1600 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® G5564 TPC-ET  (Unverified Data**)
Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon ..
Tensile Stress 11.0 MPa

@Strain 300 %
1600 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 11.0 MPa

@Strain 300 %
1600 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G45D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress >= 11.0 MPa

@Strain 300 %
>= 1600 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 285A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress >= 11.0 MPa

@Strain 100 %
>= 1600 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 298A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech