Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 83.11 MPa @Strain 3.32 %, Temperature 150 °C |
12050 psi @Strain 3.32 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc.. |
|||
Tensile Stress | 83.07 MPa @Strain 5.65 %, Temperature -40.0 °C |
12050 psi @Strain 5.65 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. .. |
|||
Tensile Stress | 83.11 MPa @Strain 0.600 %, Temperature -40.0 °C |
12050 psi @Strain 0.600 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |