Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.689 MPa @Strain 100 % |
100 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3825 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 0.689 MPa @Strain 100 % |
100 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® C4930 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 0.690 MPa @Strain 3.32 %, Temperature 200 °C |
100 psi @Strain 3.32 %, Temperature 392 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |