Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 81.0 MPa @Strain 10.0 %, Temperature 100 °C |
11700 psi @Strain 10.0 %, Temperature 212 °F |
|
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 81.0 MPa @Strain 4.00 % |
11700 psi @Strain 4.00 % |
|
Solvay TECHNYL® A 217 PA66, DRY Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim.. |
|||
Tensile Stress | 81.0 MPa @Strain 19.2 %, Temperature -40.0 °C |
11700 psi @Strain 19.2 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Tensile Stress | 81.0 MPa @Strain 0.740 %, Temperature 0.000 °C |
11700 psi @Strain 0.740 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Tensile Stress | 81.0 MPa @Strain 17.0 %, Temperature -20.0 °C |
11700 psi @Strain 17.0 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |