Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.48 MPa @Strain 100 % |
1230 psi @Strain 100 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9190 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tensile Stress | 8.48 MPa @Strain 100 % |
1230 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TL-340-S Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Stress | 8.48 MPa @Strain 0.100 %, Temperature 150 °C |
1230 psi @Strain 0.100 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon
(Unverified Data**) Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve.. |