Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.04 MPa @Strain 60.62 %, Temperature 100 °C |
1170 psi @Strain 60.62 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.04 MPa @Strain 60.62 %, Temperature 100 °C |
1170 psi @Strain 60.62 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.04 MPa @Strain 37.19 %, Temperature 120 °C |
1170 psi @Strain 37.19 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |