Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 73.0 MPa @Strain 4.00 %, Temperature 23.0 °C |
10600 psi @Strain 4.00 %, Temperature 73.4 °F |
ISO 527 |
BASF Ultrason E 3010 PES Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance. |