Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.53 MPa @Strain 36.36 %, Temperature 150 °C |
947 psi @Strain 36.36 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 6.53 MPa @Strain 46.39 %, Temperature 150 °C |
947 psi @Strain 46.39 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |