Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.18 MPa @Strain 300 % |
896 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C4945 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 6.18 MPa @Strain 17.14 %, Temperature 150 °C |
896 psi @Strain 17.14 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |