Mechanical Properties Metric English Comments
Tensile Stress 52.9 MPa

@Strain 0.810 %,
Temperature 60.0 °C
7670 psi

@Strain 0.810 %,
Temperature 140 °F
ISO 527
DuPont Performance Polymers Crastin® SK608 BK509 PBT  (Unverified Data**)
Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 52.9 MPa

@Strain 5.50 %,
Temperature 40.0 °C
7670 psi

@Strain 5.50 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr..