Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.62 MPa @Strain 100 % |
815 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3785 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 5.62 MPa @Strain 1.20 %, Temperature 90.0 °C |
815 psi @Strain 1.20 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I.. |
|||
Tensile Stress | 5.62 MPa @Strain 70.7 %, Temperature 120 °C |
815 psi @Strain 70.7 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |