Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.55 MPa @Strain 2.72 %, Temperature 90.0 °C |
805 psi @Strain 2.72 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 5.55 MPa @Strain 2.72 %, Temperature 90.0 °C |
805 psi @Strain 2.72 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 5.55 MPa @Strain 0.230 %, Temperature -20.0 °C |
805 psi @Strain 0.230 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |