Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 32.48 MPa @Strain 0.430 %, Temperature 60.0 °C |
4711 psi @Strain 0.430 %, Temperature 140 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |