Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.44 MPa @Strain 300 % |
499 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1960T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.44 MPa @Strain 75.03 %, Temperature 100 °C |
499 psi @Strain 75.03 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.44 MPa @Strain 117.8 %, Temperature 120 °C |
499 psi @Strain 117.8 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.44 MPa @Strain 0.230 %, Temperature 0.000 °C |
499 psi @Strain 0.230 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.44 MPa @Strain 77.33 %, Temperature 120 °C |
499 psi @Strain 77.33 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |