Mechanical Properties Metric English Comments
Tensile Stress 3.20 MPa

@Strain 300 %
464 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S EH 70A-3S7004 Thermoplastic Elastomer (TPE)
OnFlex™-S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t..
Tensile Stress 3.20 MPa

@Strain 300 %
464 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3653T TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 3.20 MPa

@Strain 100 %
464 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3870 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 3.20 MPa

@Strain 10.0 %,
Temperature 23.0 °C
464 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® 4069 TPC-ET  (Unverified Data**)
Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection..
Tensile Stress 3.20 MPa

@Strain 10.0 %
464 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 3.20 MPa

@Strain 10.0 %
464 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 3.20 MPa

@Strain 300 %
464 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G60A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G60A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 3.20 MPa

@Strain 300 %
464 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G60A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G60A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Copyright © lookpolymers.com All Rights Reserved