Mechanical Properties Metric English Comments
Tensile Stress 3.16 MPa

@Strain 300 %
458 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® S4740 TPE, PS Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong ..
Tensile Stress 3.16 MPa

@Strain 27.05 %,
Temperature 100 °C
458 psi

@Strain 27.05 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 3.16 MPa

@Strain 22.47 %,
Temperature 100 °C
458 psi

@Strain 22.47 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 3.16 MPa

@Strain 17.48 %,
Temperature 90.0 °C
458 psi

@Strain 17.48 %,
Temperature 194 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
Tensile Stress 3.16 MPa

@Strain 5.00 %,
Temperature 23.0 °C
458 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin..
Copyright © lookpolymers.com All Rights Reserved