Mechanical Properties Metric English Comments
Tensile Stress 24.56 MPa

@Strain 2.58 %,
Temperature 90.0 °C
3562 psi

@Strain 2.58 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It..
Tensile Stress 24.56 MPa

@Strain 2.58 %,
Temperature 90.0 °C
3562 psi

@Strain 2.58 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati..
Tensile Stress 24.56 MPa

@Strain 0.220 %,
Temperature 40.0 °C
3562 psi

@Strain 0.220 %,
Temperature 104 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)
Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance ..