Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 23.84 MPa @Strain 0.400 %, Temperature 100 °C |
3458 psi @Strain 0.400 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon
(Unverified Data**) Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve.. |
|||
Tensile Stress | 23.84 MPa @Strain 10.69 %, Temperature 40.0 °C |
3458 psi @Strain 10.69 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide.. |