Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.64 MPa @Strain 6.00 %, Temperature 40.0 °C |
383 psi @Strain 6.00 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.64 MPa @Strain 0.0500 %, Temperature -20.0 °C |
383 psi @Strain 0.0500 %, Temperature -4.00 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66
(Unverified Data**) Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in.. |
|||
Tensile Stress | 2.64 MPa @Strain 5.63 %, Temperature 90.0 °C |
383 psi @Strain 5.63 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |