Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.56 MPa @Strain 300 % |
371 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P2655 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.56 MPa @Strain 50.0 % |
371 psi @Strain 50.0 % |
Average; ASTM D412 Method A |
Seals Eastern 5794 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Tensile Stress | 2.56 MPa @Strain 0.200 %, Temperature 100 °C |
371 psi @Strain 0.200 %, Temperature 212 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 2.56 MPa @Strain 129.46 %, Temperature 120 °C |
371 psi @Strain 129.46 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.56 MPa @Strain 26.22 %, Temperature 120 °C |
371 psi @Strain 26.22 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |