Tensile Stress 2.25 MPa

@Strain 300 %
326 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® C4945E TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 2.25 MPa

@Strain 134.64 %,
Temperature 100 °C
326 psi

@Strain 134.64 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 2.25 MPa

@Strain 134.64 %,
Temperature 100 °C
326 psi

@Strain 134.64 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers