Polymer Property : Tensile Stress = 2.20 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 2.20 MPa

@Strain 300 %
319 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S EH 50A-3S7002 Thermoplastic Elastomer (TPE)
OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t..
Tensile Stress 2.20 MPa

@Strain 100 %
319 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE)
OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p..
Tensile Stress 2.20 MPa

@Strain 300 %
319 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S KG 40A-3S2016 Thermoplastic Elastomer (TPE)
OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p..
Tensile Stress 2.20 MPa

@Strain 16.44 %,
Temperature 120 °C
319 psi

@Strain 16.44 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 2.20 MPa

@Strain 300 %
319 psi

@Strain 300 %
ASTM D412
ExxonMobil Vistamaxx™ 6102 Propylene-based Elastomer
Product Description: Vistamaxx 6102 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i..
Tensile Stress 2.20 MPa

@Strain 300 %
319 psi

@Strain 300 %
ASTM D412
ExxonMobil Vistamaxx™ 6102FL Propylene-based Elastomer - Performance Film
Product Description: Vistamaxx 6102FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us..
Tensile Stress 2.20 MPa

@Strain 6.30 %,
Temperature 60.0 °C
319 psi

@Strain 6.30 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 2.20 MPa

@Strain 8.92 %,
Temperature 90.0 °C
319 psi

@Strain 8.92 %,
Temperature 194 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
Tensile Stress 2.20 MPa

@Strain 100 %
319 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G65A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G65A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.20 MPa

@Strain 100 %
319 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G65A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G65A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.20 MPa

@Strain 100 %
319 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.20 MPa

@Strain 100 %
319 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress >= 2.20 MPa

@Strain 100 %
>= 319 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 370A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress 2.20 MPa

@Strain 0.100 %,
Temperature 23.0 °C
319 psi

@Strain 0.100 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66  (Unverified Data**)
36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan..
Copyright © lookpolymers.com All Rights Reserved