Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.00 MPa @Strain 300 % |
290 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S EH 40A-3S7001 Thermoplastic Elastomer (TPE) OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tensile Stress | 2.00 MPa @Strain 300 % |
290 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S HF 50A-3S1981 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tensile Stress | 2.00 MPa @Strain 100 % |
290 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3755 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.00 MPa @Strain 100 % |
290 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Monprene® MP-1881B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.00 MPa @Strain 0.643 %, Time 3.60e+7 sec |
290 psi @Strain 0.643 %, Time 10000 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 2.00 MPa @Strain 0.557 %, Time 3600 sec |
290 psi @Strain 0.557 %, Time 1.00 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 2.00 MPa @Strain 0.641 %, Time 360000 sec |
290 psi @Strain 0.641 %, Time 100 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 2.00 MPa @Strain 0.614 %, Time 36000 sec |
290 psi @Strain 0.614 %, Time 10.0 hour |
isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 2.00 MPa @Strain 0.000 %, Temperature 23.0 °C |
290 psi @Strain 0.000 %, Temperature 73.4 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |
|||
Tensile Stress | 2.00 MPa @Strain 0.305 %, Time 3.60e+7 sec |
290 psi @Strain 0.305 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.00 MPa @Strain 0.239 %, Time 3.60e+6 sec |
290 psi @Strain 0.239 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.00 MPa @Strain 0.1575 %, Time 3600 sec |
290 psi @Strain 0.1575 %, Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.00 MPa @Strain 0.183167 %, Time 36000 sec |
290 psi @Strain 0.183167 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.00 MPa @Strain 0.224 %, Time 360000 sec |
290 psi @Strain 0.224 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.00 MPa @Strain 0.278833 %, Time 3.60e+6 sec |
290 psi @Strain 0.278833 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.00 MPa @Strain 0.355833 %, Time 3.60e+7 sec |
290 psi @Strain 0.355833 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.00 MPa @Strain 0.200 %, Time 36000 sec |
290 psi @Strain 0.200 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.00 MPa @Strain 0.235 %, Time 360000 sec |
290 psi @Strain 0.235 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.00 MPa @Strain 0.280 %, Time 3.60e+6 sec |
290 psi @Strain 0.280 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.00 MPa @Strain 0.342 %, Time 3.60e+7 sec |
290 psi @Strain 0.342 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66
(Unverified Data**) Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.00 MPa @Strain 100 % |
290 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G60A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G60A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.00 MPa @Strain 100 % |
290 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 4060A Thermoplastic Polyurethane Elastomer Zythane™ 4060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 2.00 MPa @Strain 100 % |
290 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 2.00 MPa @Strain 100 % |
290 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G60A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G60A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | >= 2.00 MPa @Strain 100 % |
>= 290 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 570A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Stress | >= 2.00 MPa @Strain 300 % |
>= 290 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 665A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | 2.00 MPa @Strain 100 % |
290 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 4070A Thermoplastic Polyurethane Elastomer Zythane™ 4070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |