Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 17.5 MPa @Strain 2.53 %, Temperature 150 °C |
2540 psi @Strain 2.53 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Tensile Stress | 17.5 MPa @Strain 0.530 %, Temperature 120 °C |
2540 psi @Strain 0.530 %, Temperature 248 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 17.5 MPa @Strain 50.0 % |
2540 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® CM600-V TPC-ES FR Extrusion, Flame Retardant (Halogen free) |
|||
Tensile Stress | 17.5 MPa @Strain 0.250 %, Temperature 23.0 °C |
2540 psi @Strain 0.250 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |